Electroplating Machined Parts: Chrome, Nickel and Zinc Options

Which finish should a buyer specify on a machined steel drawing: chrome, nickel, or zinc? Each bath solves a different problem, and choosing by appearance alone usually leads to a part that fails the salt-spray test or costs more than the function justifies. Electroplating builds a metal layer onto a machined part by suspending it in a chemical bath and running current through the solution, with the part acting as one electrode and the plating metal as the other. Over twenty to forty minutes a layer measured in microns grows onto the surface. That layer stops corrosion, changes the visible look, and in some cases adds hardness or wear resistance. The three baths buyers ask about most are chrome, nickel, and zinc, and none of them substitutes cleanly for another.

What plating actually changes on a machined part

A freshly machined steel surface sits around Ra 1.6 to 3.2 after turning or milling. Plating does not smooth it the way polishing does; it follows the existing roughness and slightly raises it. A five-micron nickel layer adds 2.5 microns to each opposing surface, so every dimension on the drawing grows.

That dimension shift matters for a 10 h7 bore that must remain h7 after plating. Designers either plate first and finish the critical feature afterward by grinding or honing, or call out the dimension as post-plate. Threads form the classic trap: a standard tapped thread plated to eight microns will not assemble unless the tap size adjusts for the build-up, which is why shops usually plate before final tapping. Reviewing which dimensions must hold after plating before the parts enter the bath prevents fit failures on arrival.

How chrome plating behaves on shafts and wear surfaces

Decorative chrome is almost never chrome alone. It applies a flash of chromium, 0.25 to 0.5 micron, over a nickel layer of ten to twenty microns. The nickel performs the corrosion work; the thin chrome on top supplies the bright, cool finish and resists fingerprinting.

Hard chrome differs from that decorative system. It deposits directly at twenty to one hundred microns, measures 700 to 1000 HV, and serves hydraulic rods, mold surfaces, and wear pads. The trade-off lies in cost and distortion: hard chrome baths run at high current density and can throw 0.02 to 0.05 mm of build-up onto sharp edges that then need grinding back. The bath does not cover recesses evenly, so deep bores and internal corners end up thinner. For a straight, visible shaft or wear surface hard chrome performs well; for a complex housing it usually proves the wrong choice. The chrome-versus-nickel comparison walks through the visual and wear trade-offs side by side.

Nickel plating for corrosion resistance and uniform coverage

Electroless nickel, the variant most shops run today, deposits five to twenty-five microns of a nickel-phosphorus alloy without external current. The alloy carries ten to twelve percent phosphorus, reaching around 500 to 600 HV as-plated and up to 1000 HV after a 400-degree C bake. It covers evenly across complex geometries, which is why manifolds and valve bodies receive this finish.

The result carries a slightly satin, uniform grey that hides underlying tool marks. Electroplated nickel, by contrast, depends on current throw and builds up faster on edges and corners. Nickel sits on the costlier end of the plating menu, typically adding twenty to forty percent to a small steel part, yet it survives 240 to 1000 hours in neutral salt spray depending on thickness. For components living in wet or chemical environments, electroless nickel becomes the default choice. The dedicated electroless nickel guide covers the bake schedule and thickness callouts in detail.

Zinc plating as the low-cost steel workhorse

Zinc fills the cheap, fast position on the menu. A five to twelve micron zinc layer on low-carbon steel costs a fraction of chrome or nickel and ships within days. On its own it lasts twelve to forty-eight hours in salt spray before white rust appears.

The yellow or clear chromate conversion that follows pushes that performance to ninety-six to two hundred hours, and a zinc-nickel alloy at twelve to fifteen percent nickel reaches five hundred to one thousand hours with a thin passivate. Zinc carries a utilitarian rather than bright-chrome appearance. It suits brackets, fasteners, and internal hardware where corrosion protection matters but cosmetics do not, and it becomes the wrong choice outdoors on visible parts because zinc tarnishes and chromate colors fade under UV exposure. Zinc-nickel, covered in the dedicated guide, is the modern upgrade for under-hood and outdoor use.

Which thickness and post-plate tolerance to call out

A drawing that names only the plating type leaves the shop to choose thickness, and that choice changes both protection and fit. Call out the micron range expected for each face, distinguish visible from hidden surfaces, and mark any critical diameter or bore as measured after plating rather than before. Features that must remain precise receive a note to machine or grind after the bath, while noncritical dimensions tolerate the pre-plate state.

Threaded holes require a separate note specifying whether tapping follows plating, because no single tap size clears the build-up across every bath thickness. Corner radii and recessed areas deserve a review, since current distribution thins the layer there and a stated nominal thickness may not actually reach inside.

How cost and lead time compare across the three baths

Zinc runs fastest and cheapest, suitable for large batches of brackets and fasteners where days matter. Electroless nickel occupies the middle on both axes, with uniform coverage that offsets a moderate surcharge for complex parts. Chrome, especially hard chrome paired with post-plate grinding, carries the highest cost and the longest schedule, driven by preparation, edge build-up, and the finishing operation required after plating.

Buyers often underestimate the secondary work: a hard-chromed rod that needs cylindrical grinding returns to the machine shop after the bath, and that step adds hours and tolerance work not reflected in the plating quote alone. Ask the plater and machining shop to coordinate whether finish machining occurs before or after plating, so the two operations share one final dimension rather than working against each other.

Compliance, chromate, and market restrictions

Whatever finish the design picks, the supplier must know which market receives the parts. Hexavalent chromate remains restricted under most RoHS and REACH frameworks, while trivalent alternatives and zinc-nickel passivation satisfy those rules on most shipments. Tell the shop whether RoHS or REACH compliance matters for the destination market before the quote locks in a chromate system.

Documentation often accompanies that statement: coating thickness certificates and salt-spray reports keep an audit trail for automotive and export customers.

Matching the finish to visible role, corrosion load, and sliding contact

A few questions narrow the field efficiently. Is the part visible? A bright mirror look calls for decorative chrome over nickel; a visible but satin grey finish accepts electroless nickel. Is the component hidden inside a machine but required not to rust? Zinc with a clear or yellow chromate answers on cost, while zinc-nickel handles damp or salty environments. Does one surface slide against another? Hard chrome at twenty to fifty microns or baked electroless nickel near 1000 HV supplies the wear answer, with post-plate grinding expected.

Mark plating thickness and post-plate tolerance on the drawing, name the chromate type, and call out any critical dimension machined after plating. The surface finishing guide lists trade-offs between plating, anodizing, and powder coat when the part material is aluminum rather than steel.

⚙