Which engineering plastic should a seal or bearing choose: PTFE, PEEK, or POM? Seals and bearings ask three questions of a material: will it hold its shape under load, will it survive the temperature and chemicals it contacts, and will it run without galling against a metal shaft. PTFE, PEEK, and POM each win one of those contests and lose another. PTFE dominates friction and chemistry yet disappoints structurally, PEEK carries the high-temperature workhorse role at premium pricing, and POM, also called acetal, stands as the cheap stiff default for everyday bearing work. The choice usually comes down to which failure mode the application cannot tolerate rather than which plastic ranks best overall.
Which plastic handles ordinary room-temperature bearings
Acetal, sold under trade names including Delrin, forms the starting point for bushings, thrust washers, and seal carriers sitting near room temperature. It holds a bearing-type tolerance well, machines cleanly on standard tooling, and costs a fraction of PEEK.
Its limiting factors are heat and hot water: POM keeps useful properties to about 80 to 100 °C continuously, and it creeps slowly under sustained load, so a bushing pressed in place and loaded indefinitely relaxes over time. Moisture uptake stays low, which keeps dimensions stable in normal humidity. For a low-load bearing running against a hardened shaft at room temperature, POM remains the answer, with the best machining economics of the three. The acetal POM machining guide covers the feeds and tooling that prevent chipping.
POM performs best against a smooth, hardened shaft; a rough or unhardened steel surface abrades the polymer faster than the bearing design expects, and a poorly lubricated bushing generates heat that pushes the material past its modest temperature ceiling. Its dimensional stability also suits molded-in-place carrier plates, spacers, and snap-fit parts where consistent wall thickness matters, though sustained compression against a hot surface will gradually relax the press fit. Buyers matching POM to a bearing should state shaft hardness, expected load, and whether the environment stays dry or sees periodic lubrication, since those conditions determine whether the bushing wears predictably or fails early.
Why PTFE wins on friction and chemical resistance
PTFE is the material reached for when nothing else survives the fluid. It is nearly chemically inert, runs from minus 200 to plus 260 °C, and carries the lowest coefficient of friction of any engineering plastic, around 0.1 against steel, which makes it the classic seal face and gland packing material.
The trade-off is structural. PTFE stays soft, cold-flows under load, and does not hold tight dimensions; a PTFE bushing cannot carry the same load as a POM one, and tolerances on machined PTFE loosen to about ±0.05 to 0.1 mm because the material deflects under contact. It also machines poorly, producing gummy chips and a tendency to shift, which is why shops take light cuts with sharp tooling and often fill it with glass, carbon, or bronze to stiffen the plain resin. The dedicated PTFE machining write-up goes into those limits in detail.
What PEEK brings under heat and sustained load
PEEK occupies the gap between the two extremes. It runs to about 250 °C continuously, retains strength under load far better than PTFE, machines to tight tolerances, and resists most chemicals seen in oil-and-gas and semiconductor service. It suits bearing retainers, seal rings, and wear pads that see real load alongside real heat.
The catch is price: PEEK bar stock costs roughly five to ten times POM, and it demands carbide tooling and rigid setups because glass- or carbon-filled grades stay stiff and abrasive. Unfilled PEEK eases tool wear but proves weaker; filled grades grow stronger yet wear cutters faster. For a seal or bearing that must survive 150 °C and a hydrocarbon fluid, PEEK is usually the only one of the three that answers. The practical PEEK machining tips guide spells out the required setup discipline.
Semiconductor and downhole environments push PEEK further than general industrial service: components sit near hot fluids, vacuum conditions, or repeated thermal cycling where creep under clamp load cannot be tolerated. In those settings PEEK often replaces metal retainers and wear rings to save weight and avoid corrosion, while its ability to hold a machined bore over long periods keeps alignment stable. Because the resin absorbs little moisture and resists hydrolysis better than POM, it also survives steam and hot-water exposure that would weaken acetal over time. The trade-off remains cost and cycle time: PEEK blanks carry a high material price, and shops machine them more slowly to protect dimensions and avoid internal stress.
Side-by-side numbers on temperature, strength, and tolerance
Comparing the three side by side makes the differences concrete. POM handles about 80 to 100 °C continuously and cuts to ±0.02 to 0.05 mm at the lowest material cost. PTFE handles up to 260 °C and the widest chemical range, yet its compressive strength stays low and tolerances loosen to about ±0.1 mm because it creeps under pressure. PEEK handles 250 °C, retains bearing-level strength under load, cuts tightly, and costs the most of the group.
Friction ranking places PTFE lowest, POM in the middle, and PEEK higher again, which explains why PEEK bearings often run with a PTFE liner or grease rather than dry contact. Filled grades of PEEK and acetal wear tools faster and return slightly looser dimensions, so the drawing should state whether the filled version applies. A machined seal ring frequently needs a light hand-feed finish on the sealing lip, because a tool mark there becomes a leak path once pressure is applied. When the application is a rotating seal ring in a hot hydrocarbon, the PEEK versus PTFE trade-off matches the exact decision buyers face.
Matching the material to fluid, heat, and shaft speed
Selection starts with continuous operating temperature. Under 80 °C in ordinary fluids, POM almost always wins on cost and machinability; above that range, or in aggressive chemicals, the material moves up the scale. When the priority is low friction and chemical resistance with a light load, PTFE or a filled PTFE earns the call; when the part carries load and heat and must hold a bore over years, PEEK becomes the honest choice.
Telling the shop the fluid, operating temperature, and shaft speed on the drawing decides the material more than price alone. Expect PEEK and PTFE to cost more and take longer than POM, since both need special tooling and careful feeds. Oil-and-gas and semiconductor buyers often end up with PEEK seals paired with PTFE backup rings, combining load capacity from one polymer with sliding performance from the other. Matching each plastic to the job it actually performs avoids over-specifying a premium resin where POM suffices, and avoids under-specifying POM where heat or chemistry would quickly degrade it.