Chemical Conversion Coating (Chem Film): Basics for Aluminum

Chemical conversion coating — also called chem film, chromate conversion coating, Alodine, or Iridite — is one of the thinnest, cheapest ways to protect a machined aluminum part. A treated bracket or housing keeps its dimensions, stays electrically conductive, and takes paint or powder better than bare aluminum. It is not anodizing and it is not plating. The coating forms when a chromate or chromium-free solution reacts with the aluminum surface and deposits a thin, adherent film in minutes. For a buyer it is worth understanding because it changes how a part tolerates salt spray, how it accepts paint, and how much the quote moves.

What the coating actually is

Bare aluminum builds a natural oxide layer, but that layer is soft, patchy, and does not seal the surface well. Chem film speeds that reaction under controlled conditions. The part is degreased, often acid-etched for a few seconds, then dipped or sprayed with the conversion solution. Over 1 to 5 minutes the solution converts a few micrometers of the aluminum surface into a mixed oxide-chromate film that bonds chemically rather than sitting on top. The result lands at roughly 0.5 to 3 grams per square meter, which translates to about 0.1 to 0.5 micrometers of thickness. Because it is that thin, a bore machined to +0.005 mm does not need rework after coating — the film does not move the dimension the way anodizing can, because anodize builds up 5 to 25 micrometers on every surface.

Corrosion protection and electrical grounding

The film does two jobs at once. First it seals the aluminum against humidity and salt spray. A properly coated 6061 panel commonly passes 168 hours of neutral salt spray under ASTM B117 without pitting, and many specs write that number straight onto the drawing. Second, and this is why electronics buyers ask for it by name, the coating stays conductive. Anodizing electrically insulates a housing, which kills a grounding path from the mounting face to the PCB shield. Chem film lets that path survive. That is the reason radio, telecom, and enclosure parts are often chem-filmed instead of anodized even though anodize looks cleaner. Our surface finishing guide lays out the whole finishing menu, and the anodizing guide shows when anodize is the better call.

The two spec classes and what they cost

Buyers usually meet chem film through MIL-DTL-5541, which splits the coating into Class 1 and Class 3. Class 1 uses hexavalent chromate and gives the best salt-spray performance with the lowest contact resistance. Hexavalent chromium is restricted under RoHS and REACH, though, so most commercial work now runs Class 3 chromium-free. Class 3 delivers around 96 to 168 hours of salt spray depending on alloy and pretreatment — close enough for most enclosures, and fully compliant. Type I and Type II in the same spec refer to whether the part will also be painted. Color is not a quality signal: chem film ranges from colorless to light gold, and a stronger gold tint does not mean a thicker or better coating. Treat the color as cosmetic and read the test report instead.

Where chem film stops being the answer

Three limits come up on the shop floor. Wear is the first. Chem film is soft, roughly the hardness of a thick paint film, so sliding surfaces, threads that see repeated assembly, and sealing faces wear through in a handful of cycles. Machine those features to final size after coating, or mask them off. The second limit is appearance. Chem-filmed aluminum looks dull or faintly blotchy, and machined tool marks show straight through; if the part is visible, bead blasting before coating, or a clear anodize after, reads far better. The third limit is pretreatment. Castings and extrusions that carry release agent or heavy oxide need proper cleaning, or the film rubs off on first handling. For visible cosmetic parts, a clear coat over anodizing usually wins, and our clear coat guide walks through that trade-off.

Specifying chem film so the quote is clean

Put three things on the drawing and the quote comes back the first time: the spec (for example MIL-DTL-5541 Type II Class 3, or a chromate-free equivalent), the required salt-spray hours, and which surfaces must stay uncoated. Call out tapped holes and mating bores as mask-mandatory unless you accept touch-up afterward. Ask for a cell-test or coating-weight report when the part carries a ground, because contact resistance above 1 milliohm later shows up as an intermittent grounding fault nobody can trace. A typical chem film batch adds USD 0.5 to 3 per part plus a process fee of USD 40 to 120, and it usually adds one to two days because most shops send it out rather than tank it in-house. Done right, it is the cheapest corrosion and grounding upgrade a machined aluminum part can get. If you are still picking the alloy, our aluminum machining guide grades the common choices before you decide on the finish.

⚙