Delrin vs Nylon for Machined Parts: What’s Better?

A plastic gear sits inside a packaging machine that ran fine through the dry winter months, then starts binding six months later once humidity climbs. The bore has swollen, the tooth lash changed, and the buyer faces the same question behind dozens of failed plastic parts: was the grade wrong all along? Delrin, the acetal also sold as POM, and nylon, usually PA6 or PA66, occupy the same slot in every engineering plastic catalog. Neither is universally the better machined plastic. Delrin protects dimensional stability and tight tolerance; nylon protects toughness, wear, and load capacity. The comparison below separates what each material does well so the choice matches the part before the failure shows up in service.

Two materials, two very different baselines

Delrin 150 is a homogeneous acetal copolymer with tensile strength around 60 to 70 MPa and a flexural modulus near 3,000 MPa. It absorbs almost no water, below a 0.2 percent saturation level, which means a part machined on Tuesday measures the same the following August. Nylon 66 reaches a similar tensile strength of 80 to 90 MPa but flexes more, with a modulus around 2,800 to 3,000 MPa, and it is hygroscopic: it picks up 1.5 to 3 percent moisture from the air, swelling the part and shifting its dimensions over time.

Read that as a split in character rather than a winner. Nylon is the tougher, more forgiving material; Delrin is the stiffer, more predictable one. The acetal POM machining guide covers how Delrin cuts, while the nylon CNC machining guide walks through the PA grades buyers most often specify.

Tolerance drift separates them most clearly

This is usually where the decision settles. A Delrin part holds ±0.05 mm across a feature under normal shop conditions, because nothing moves after machining. A nylon part starts at that accuracy the day it leaves the machine, then drifts. A 50 mm bore in nylon can shift 0.08 to 0.15 mm as the material absorbs ambient moisture over several weeks. That movement suits a snap bracket but disqualifies a locating pin.

Shops compensate by machining nylon from stress-relieved, pre-conditioned blanks and letting the part equilibrate before the final bore, but the baseline drift never disappears completely. When the drawing calls for a press fit or a sliding clearance that must hold steady across seasons, Delrin is the safer call. Our side-by-side Delrin versus nylon breakdown shows the fit numbers buyers most frequently misread during selection.

Wear, friction, and impact in service

Nylon pulls ahead against a moving surface. It runs dry against steel with a low coefficient of friction and wears slowly, which is why gears, bearing blocks, and packaging star wheels are usually nylon. Glass-filled nylon, PA66-GF30, raises the modulus to 6,000 to 8,000 MPa and cuts wear further, though the glass fibers abrade tooling faster.

Delrin also runs well and carries the lower friction coefficient, around 0.2 to 0.3 against steel, but it resists impact less and can crack under repeated shock. A lightly loaded, dimension-critical spacer leans toward Delrin; a gear tooth that takes torque and repeated impact leans toward nylon. Glass-filled nylon demands a sharper tool and shorter tool life, so the per-piece price reflects that abrasion, while unfilled nylon stays gentler on the cutters. At similar wall thicknesses nylon also runs slightly lighter than acetal. The difference shows in how the part moves under load, not in how it behaves on the machine, so evaluate the duty cycle rather than only the strength rating.

How each cuts, and when to combine both

Both plastics prefer sharp, positive-rake tools and moderate spindle speeds, but they chip differently. Delrin breaks into clean, brittle chips and produces the best surface finish of any common engineering plastic, which makes it the default for precision housings and visible parts. Nylon is tougher and more ductile; it strings and smears once the edge dulls, and it deflects more under the cutter, so thin walls need support and lighter feeds. Coolant stays optional on Delrin, usually run dry with an air blast, while nylon machines cleanly with either approach. For the broader shortlist of PEEK, PTFE, and other grades, the plastic machining guide covers how each one compares.

Setup decisions follow the same split. Delrin tolerates a more aggressive clamp because it resists creep under steady pressure; nylon held too tightly deforms during the cut and springs back after unclamp, so it needs softer jaws, full support under the wall, and a light finishing pass after the part settles. When nylon will sit inside a humid enclosure or near a wet process, ask the shop to size bores and slots with that swelling in mind, rather than expecting the as-machined dimension to remain fixed in service.

Choose Delrin when the part must hold a tight dimension through humidity, stay visible, or achieve the cleanest finish. Choose nylon when the part carries sliding wear, impact, or repeated torque, and when a dimension that settles after machining is acceptable. If a single component needs both tight tolerance and high wear, the answer often combines the two: a Delrin body with a nylon wear insert, or a glass-filled nylon bore with a Delrin locating face. Always name the exact grade on the drawing, because Delrin 150 and Delrin 570, or PA6 versus PA66-GF30, machine and measure differently. Note the operating temperature and whether the part sees moisture, then let the shop flag the grade that fits before quoting.

⚙

Ready to Start Your CNC Project?

Get a free quote within 24 hours. ISO 9001 certified, 20+ years experience, low-volume friendly from 1 piece.

Get a Quote